Tag: Niobium in Superalloys

The Role of Niobium in Superalloys

0 Comment

The Role of Niobium in Superalloys Refractory elements are important alloying additions in both nickel-base and iron-nickel-base superalloys. They are responsible for the increased high-temperature mechanical properties present in current superalloy systems. In this article, we’ll take a look at the role of niobium in superalloys. It has long been established that nickel-base and iron-nickel-base […]

Tags: , , , , , , ,